Final coat apply
Finally, the final coats are applied. I used Target EMM6000 water based acrylic finish. Last time, I used the EMM7000HB with some troubles. EMM6000 is so much easy to control for me. This time, I have gotten very satisfied results, and I am pretty happy. Two guitars need two weeks to cure the finishing, and then I will take surfacing and polishing.
Sunday, October 6, 2013
Epoxy filler sanding and Yellow stain apply
Sanding for the Epoxy filler is done. I did two sessions for the neck filler apply, and one session for the body and the top. After finishing the sanding session, I applied Yellow stain on top for both models. Yellow stain is very light color; however, it is enough to make an impressive beauty.